Characteristic |
ASTM # # |
Result |
| Specific Gravity |
|
1.2 to 1.9 depending on color. |
| Theoretical Coverage |
|
Approximately 101 to 160 ft.2 / lb. / mil. |
| Optimum Storage |
|
<80° F, < 50%RH |
| Particle Distribution |
|
+44 microns (325 mesh). Percentage varies with color. |
| Film Thickness |
D-1186 |
Recommended, 2 to 6 mils. |
| Percent Gloss @ 60° |
D-523-89 |
25 to 95+ |
| Pencil Hardness |
D-3363-00 |
H to 3H |
| Adhesion |
D-3359-02 |
No lifting of 1/8" squares between scribed lines when |
|
|
cross hatch adhesion is tested using the prescribed tape. |
| Flexibility |
D-522-93a |
A coating of 2 mils or less will withstand a bend of 180° |
|
|
over a 1/8" mandrel without cracking or loss of adhesion. |
| Impact Resistance |
D-2794-93 |
160 inch-pounds, direct and reverse, at a
film thickness of 2 mils. |
|
|
Impact will be influenced by formulation. |
| Salt Spray Resistance |
B-117-97 |
Less than 1/16" undercoating after 1000 hours of exposure |
|
|
1000 hours of exposure in 5% salt spray at 95° F and 95% relative humidity. |
| Overbake |
|
Polyesters can typically withstand 200% overbake without yellowing |
| Weatherability |
|
After 1 year of South Florida sun exposure, coatings exhibit a a minimal loss of gloss |
|
|
and no deterioration. Super Durable polyesters are available. |
|